Troubleshooting

Voids in part

Return to Troubleshooting Guide (click here)

Possible Cause Possible Solution
Material in core sets up more
slowly than surface material,
especially in thick cross sections.
Increase injection pressure and time.       Increase back pressure.                         Increase mold temperature.
Make sure sprue, runner and gates are
are large enough to assure free flow.
Increase cooling time.
There is moisture in pellets (raw material) Pre-dry material/pellets according to instructions.